1.1 This test method establishes procedures for the determination of the reversed or repeated bending fatigue properties of copper alloy flat-sheet or strip-spring materials by fixed cantilever, constant deflection (that is, constant amplitude of displacement)-type testing machines. This method is limited to flat stock ranging in thickness from 0.005 to 0.062 in. (0.13 to 1.57 mm), to a fatigue-life range of 105 to 108 cycles, and to conditions where no significant change in stress-strain relations occurs during the test.
Note 1: This implies that the load-deflection characteristics of the material do not change as a function of the number of cycles within the precision of measurement. There is no significant cyclic hardening or softening.
| Author | ASTM |
|---|---|
| Editor | ASTM |
| Document type | Standard |
| Format | File |
| Confirmation date | 2009-04-01 |
| ICS | 77.150.30 : Copper products |
| Number of pages | 5 |
| Replace | ASTM B593-96(2009)e1 |
| Set | ASTMVOL0201 |
| Year | 2009 |
| Document history | ASTM B593-96(2009)e1 |
| Country | USA |
| Keyword | ASTM 593;ASTM B593;ASTM B593;10.1520/B0593-96R14E01 |