No products
View larger New product
1.1 This test method was developed using copper electrodes to evaluate the low-voltage (up to 600 V) tracking resistance of materials in the presence of aqueous contaminants.2
Note 1: At this time, only industrial laminates have been examined using this method, which was developed at the National Manufacturers Electrical Association (NEMA) laboratory located at the University of Cincinnati. It was found that a closer end point (less scatter) was obtained than with platinum electrodes, and materials tested tended to be ranked by resin system.
| Author | ASTM |
|---|---|
| Editor | ASTM |
| Document type | Standard |
| Format | File |
| ICS | 29.035.01 : Insulating materials in general |
| Number of pages | 5 |
| Replace | ASTM D5288-10 |
| Set | ASTMVOL1002 |
| Year | 2014 |
| Document history | ASTM D5288-10 |
| Country | USA |
| Keyword | ASTM 5288;ASTM D5288;ASTM D5288;10.1520/D5288-14 |