1.1 This test method2 covers the determination of the average force to propagate tearing through a specified length of plastic film or nonrigid sheeting after the tear has been started, using an Elmendorf-type tearing tester. Two specimens are cited, a rectangular type, and one with a constant radius testing length. The latter shall be the preferred or referee specimen.
| Author | ASTM |
|---|---|
| Editor | ASTM |
| Document type | Standard |
| Format | File |
| ICS | 83.140.10 : Films and sheets |
| Number of pages | 7 |
| Replace | ASTM D1922-09 |
| Set | ASTMVOL0801 |
| Year | 2015 |
| Document history | ASTM D1922-09 |
| Country | USA |
| Keyword | ASTM 1922;ASTM D1922;ASTM D1922;10.1520/D1922-15 |