1.1 Under certain conditions of stress, and in the presence of environments such as soaps, wetting agents, oils, or detergents, blow-molded polyethylene containers exhibit mechanical failure by cracking at stresses appreciably below those that would cause cracking in the absence of these environments.
| Author | ASTM |
|---|---|
| Editor | ASTM |
| Document type | Standard |
| Format | File |
| ICS | 83.080.20 : Thermoplastic materials 83.140.99 : Other rubber and plastics products |
| Number of pages | 7 |
| Replace | ASTM D2561-12 |
| Set | ASTMVOL0801 |
| Year | 2017 |
| Document history | ASTM D2561-12 |
| Country | USA |
| Keyword | ASTM 2561;ASTM D2561;ASTM D2561;10.1520/D2561-17 |