1.1 This practice covers the determination of a degradation-end point (a brittle point) for degradable polyethylene/polypropylene films and sheeting less than 1.0 mm (0.04 in.) thick. This practice is not intended for determination of the rate or degree of degradation of a polyethylene/polypropylene film or sheet, but rather, to assess when in the course of its degradation under some condition, a brittle point is reached. If one wishes to monitor tensile elongation during the degradation process (such as when the tensile elongation is significantly greater than 5 %), Test Method D882 is recommended. This practice is not to be considered the only way of determining a degradation-end point.
| Author | ASTM |
|---|---|
| Editor | ASTM |
| Document type | Standard |
| Format | File |
| ICS | 83.140.01 : Rubber and plastics products in general |
| Number of pages | 4 |
| Replace | ASTM D3826-98(2013) + Redline |
| Set | ASTMVOL0802 |
| Year | 2018 |
| Document history | ASTM D3826-98(2013) + Redline |
| Country | USA |
| Keyword | ASTM 3826;ASTM D3826;ASTM D3826;10.1520/D3826-18 |