Could I help you?
New Sale! View larger

ASTM E3039-18 + Redline

New product

ASTM E3039-18 + Redline

Standard Test Method for Determination of Crack-Tip-Opening Angle of Pipe Steels Using DWTT-Type Specimens

More details

$23.65

-57%

$55.00

More info

1.1 This test method covers the determination of fracture propagation toughness in terms of the steady-state crack-tip-opening angle (CTOA) using the drop-weight tear test (DWTT)-type specimen. The method is applicable to pipe steels that exhibit predominantly ductile fracture with at least 85% shear area measured according to Test Method E436 - Standard Test Method for Drop-Weight Tear Tests of Ferritic Steels. This test method applies to steel pipes with wall thicknesses between 6 mm and 20 mm. Annex A1 describes the method to test pipe steels with wall thickness between 20 mm to 32 mm.

Author ASTM
Editor ASTM
Document type Standard
Format File
ICS 77.080.20 : Steels
Number of pages 9
Replace ASTM E3039-16 + Redline
Set ASTMVOL0301
Year 2018
Document history ASTM E3039-16 + Redline
Country USA
Keyword ASTM 3039;ASTM E3039;ASTM E3039;10.1520/E3039-18